Technical Specs
4701-40-15250-04
PORON® 4701-40 Polyurethane
Product Data Sheet for 4701-40-15250-04
4701401525004 |
||
PROPERTY |
VALUE |
TEST METHOD |
Density kg /m3 |
240 |
ASTM D 3574-95, Test A |
Density lb / ft3 |
15 |
|
Temperature Resistance Recommended Constant Use, max Recommended Intermit Use, max |
90°C (194°F) 121°C (250°F) |
SAE J-2236
|
Tolerance, % |
± 10 |
|
Thickness, mm |
6.35 |
|
Thickness, (inches) |
0.25 |
|
Tolerance, % |
± 10 |
|
Standard Color |
Black |
|
Compression Force Deflection, kPa |
27-76 |
0.51cm/min (0.2” / min) Strain Rate |
Compression Force Deflection, (psi) |
(4-11) |
|
Compression Force Deflection, Typical kPa, (psi) |
41 (5) |
|
Hardness, Durometer, Shore "O", |
12 |
ASTM D 2240-97 |
Hardness, Durometer, Shore “A” |
8 |
ASTM D 2240-97 |
Compression Set, % max. |
5 |
ASTM D 1667-90 Test D @ 23℃(73℉) |
Compression Set, % max. |
10 |
ASTM D 3574-95 Test D @ 70℃(158℉) |
Compression Set, % max. |
5 |
ASTM D 3574-95 Test J/Test D |
Dimensional Stability, % max. change |
± 1 |
22 hrs @ 80℃(176℉) in a forced-air oven |
Tensile Strength, kPa (psi) min. |
276 (40) |
ASTM D 3574-75 Test E |
Color |
Black |
|
Tensile Elongation, % min., |
100 |
ASTM D 3574-75 Test E |
Tear Strength, kN/m (pli) min |
0.5 (3) |
ASTM D 264-91 Die C |
Typical kN/m (pli) |
1.2 (7) |
ASTM D 264-91 Die C |
Water Absorption, Immersion Testing, % Weight Gain, Typical |
17 |
ASTM D570-95 |